  • Cross-Linking Cellulosic Fibers with Photoreactive Polymers: Visualization with Confocal Raman and Fluorescence Microscopy.

Cross-Linking Cellulosic Fibers with Photoreactive Polymers: Visualization with Confocal Raman and Fluorescence Microscopy.

Biomacromolecules (2015-06-24)
Marek Janko, Michael Jocher, Alexander Boehm, Laura Babel, Steven Bump, Markus Biesalski, Tobias Meckel, Robert W Stark
摘要

The properties of paper sheets can be tuned by adjusting the surface or bulk chemistry using functional polymers that are applied during (online) or after (offline) papermaking processes. In particular, polymers are widely used to enhance the mechanical strength of the wet state of paper sheets. However, the mechanical strength depends not only on the chemical nature of the polymeric additives but also on the distribution of the polymer on and in the lignocellulosic paper. Here, we analyze the photochemical attachment and distribution of hydrophilic polydimethylacrylamide-co-methacrylate-benzophenone P(DMAA-co-MABP) copolymers with defined amounts of photoreactive benzophenone moieties in model paper sheets. Raman microscopy was used for the unambiguous identification of P(DMAA-co-MABP) and cellulose specific bands and thus the copolymer distribution within the cellulose matrix. Two-dimensional Raman spectral maps at the intersections of overlapping cellulose fibers document that the macromolecules only partially surround the cellulose fibers, favor to attach to the fiber surface, and connect the cellulose fibers at crossings. Moreover, the copolymer appears to accumulate preferentially in holes, vacancies, and dips on the cellulose fiber surface. Correlative brightfield, Raman, and confocal laser scanning microscopy finally reveal a reticular three-dimensional distribution of the polymer and show that the polymer is predominately deposited in regions of high capillarity (i.e., in proximity to fine cellulose fibrils). These data provide deeper insights into the effects of paper functionalization with a copolymer and aid in understanding how these agents ultimately influence the local and overall properties of paper.

材料
货号
品牌
产品描述

Sigma-Aldrich
N,N-二甲基甲酰胺, for molecular biology, ≥99%
Sigma-Aldrich
罗丹明B, ≥95% (HPLC)
Sigma-Aldrich
三乙基胺, BioUltra, ≥99.5% (GC)
Sigma-Aldrich
氧化铝, nanopowder, <50 nm particle size (TEM)
Sigma-Aldrich
罗丹明B, for fluorescence
Sigma-Aldrich
二乙醚
Sigma-Aldrich
氧化铝, nanoparticles, <50 nm particle size (DLS), 20 wt. % in isopropanol
Sigma-Aldrich
二氯甲烷, anhydrous, ≥99.8%, contains 40-150 ppm amylene as stabilizer
Sigma-Aldrich
三乙基胺, ≥99.5%
Sigma-Aldrich
N,N-二甲基甲酰胺, anhydrous, 99.8%
Sigma-Aldrich
四氢呋喃, anhydrous, ≥99.9%, inhibitor-free
Sigma-Aldrich
四氢呋喃, anhydrous, contains 250 ppm BHT as inhibitor, ≥99.9%
Sigma-Aldrich
甲醇, anhydrous, 99.8%
Sigma-Aldrich
氧化铝, nanopowder, 13 nm primary particle size (TEM), 99.8% trace metals basis
Sigma-Aldrich
丙酮, natural, ≥97%
Sigma-Aldrich
氧化铝, 99.997% trace metals basis
Sigma-Aldrich
三乙基胺, ≥99%
Sigma-Aldrich
4-羟基二苯甲酮, 98%
Sigma-Aldrich
三乙基胺, for amino acid analysis, ≥99.5% (GC)
Sigma-Aldrich
氧化铝, nanoparticles, 30-60 nm particle size (TEM), 20 wt. % in H2O
Sigma-Aldrich
丙酮, ≥99%, meets FCC analytical specifications
Sigma-Aldrich
三乙基胺, for protein sequence analysis, ampule, ≥99.5% (GC)
Sigma-Aldrich
氧化铝, single crystal substrate, <0001>
Sigma-Aldrich
氧化铝, nanowires, diam. × L 2-6 nm × 200-400 nm
Sigma-Aldrich
介孔氧化铝, MSU-X (wormhole), average pore size 3.8 nm
Sigma-Aldrich
N,N-二甲基乙酰基乙酰胺 溶液, 80% in H2O
Sigma-Aldrich
三乙基胺, puriss. p.a., ≥99.5% (GC)
Sigma-Aldrich
甲醇, NMR reference standard
Sigma-Aldrich
甲醇 溶液, NMR reference standard, 4% in methanol-d4 (99.8 atom % D), NMR tube size 3 mm × 8 in.
Sigma-Aldrich
甲醇-12C, 99.95 atom % 12C