跳转至内容
Merck
CN

GF83603909

foil, 50x50mm, thickness 0.5mm, annealed, 99.2%

别名:

登录查看公司和协议定价


About This Item

经验公式(希尔记法):
Zr
CAS号:
分子量:
91.22
MDL编号:
UNSPSC代码:
12141751
PubChem化学物质编号:
NACRES:
NA.23

方案

99.2%

表单

foil

制造商/商品名称

Goodfellow 836-039-09

电阻率

40 μΩ-cm, 20°C

尺寸 × 厚度

50 x 50 mm × 0.5 mm

沸点

4377 °C (lit.)

mp

1852 °C (lit.)

密度

6.5 g/mL at 25 °C (lit.)

SMILES字符串

[Zr]

InChI

1S/Zr

InChI key

QCWXUUIWCKQGHC-UHFFFAOYSA-N

正在寻找类似产品? 访问 产品对比指南

一般描述

For updated SDS information please visit www.goodfellow.com.

法律信息

Product of Goodfellow

储存分类代码

11 - Combustible Solids

WGK

nwg

闪点(°F)

Not applicable

闪点(°C)

Not applicable

法规信息

新产品

历史批次信息供参考:

分析证书(COA)

Lot/Batch Number

抱歉,我们目前尚未线上提供该产品的COA。

如需帮助,请联系 客户支持

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

Abnormal trace metals in man: zirconium.
H A Schroeder et al.
Journal of chronic diseases, 19(5), 573-586 (1966-05-01)
Oluwatayo F Ikotun et al.
Future medicinal chemistry, 3(5), 599-621 (2011-04-30)
Positron emission tomography, with its high sensitivity and resolution, is growing rapidly as an imaging technology for the diagnosis of many disease states. The success of this modality is reliant on instrumentation and the development of effective and novel targeted
Yugo Hatai
The international journal of esthetic dentistry, 9(2), 206-222 (2014-04-26)
In contemporary dentistry, we have a vast range of materials to choose from, and metal free restorations have become the premier materials for achieving the ultimate in both esthetics and durability. Metal-free restorations are utilized with more conservative preparations to
David B N Lee et al.
ASAIO journal (American Society for Artificial Internal Organs : 1992), 56(6), 550-556 (2011-01-20)
Recent years have witnessed a rapid increase in the use of zirconium (Zr)-containing compounds in artificial internal organs. Examples include dental implants and other restorative practices, total knee and hip replacement, and middle-ear ossicular chain reconstruction. In nephrological practice, Zr-containing
Thomas J Heyse et al.
Expert review of medical devices, 9(4), 409-421 (2012-08-22)
Polyethylene wear is a key contributor to long-term failure in total knee arthroplasty. Oxidized zirconium alloy was created as a bearing surface for total joint arthroplasty in an attempt to address this concern. Oxidized zirconium has shown considerable improvements over

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门