蒸汽压
<0.01 mmHg ( 537.2 °C)
检测方案
≥99% trace metals basis
形式
nanopowder
自燃温度
572 °F
电阻率
13.5 μΩ-cm, 20°C
粒径
<25 nm (BET)
bp
5425 °C (lit.)
mp
2996 °C (lit.)
密度
16.69 g/cm3 (lit.)
SMILES字符串
[Ta]
InChI
1S/Ta
InChI key
GUVRBAGPIYLISA-UHFFFAOYSA-N
一般描述
超细颗粒的大量附聚体。
警示用语:
Danger
危险声明
危险分类
Flam. Sol. 1
WGK
nwg
闪点(°F)
Not applicable
闪点(°C)
Not applicable
International journal of nanomedicine, 15, 2419-2435 (2020-05-06)
In recent years, nanomaterials have been increasingly developed and applied in the field of bone tissue engineering. However, there are few studies on the induction of bone regeneration by tantalum nanoparticles (Ta NPs) and no reports on the effects of
Vascular, 21(2), 87-91 (2013-03-20)
Control of back bleeding from the hypogastric artery into the aneurysm after endovascular aneurysm repair (EVAR) of a ruptured aorto-iliac aneurysm may be necessary in order to avoid a type II endoleak. It is an emergency situation and selective catheterization
Journal of the mechanical behavior of biomedical materials, 16, 21-28 (2012-11-10)
Microstructure and mechanical properties of laser deposited complex quaternary Ti-34Nb-7Zr-7Ta (all wt%), an orthopedic load-bearing implant alloy, has been investigated in detail in both as-deposited as well as heat-treated (β-solutionized and quenched) conditions. The difference in stress-strain behavior of this
Orbital ultrasound in the selective screening of a dural-cavernous sinus fistula.
European journal of emergency medicine : official journal of the European Society for Emergency Medicine, 20(2), 137-139 (2013-02-26)
Nanoscale, 5(4), 1494-1498 (2013-01-23)
Ta oxide nanotubes (NTs) were formed by the anodization of Ta at 15 V in a solution of concentrated sulfuric acid containing 0.8-1.0 M hydrofluoric acid. To study the initial stages of NT formation, FESEM images of samples anodized for
我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.
联系技术服务部门