99.9% trace metals basis
形式
rod
反应适用性
reagent type: reductant
电阻率
9.446 μΩ-cm, 20°C
直径
12.7 mm
bp
1342 °C (lit.)
mp
180 °C (lit.)
密度
0.534 g/mL at 25 °C (lit.)
应用
battery manufacturing
SMILES字符串
[Li]
InChI
1S/Li
InChI key
WHXSMMKQMYFTQS-UHFFFAOYSA-N
正在寻找类似产品? 访问 产品对比指南
一般描述
我们的高纯锂棒直径为12.7 mm,是由锂制成的圆柱形金属样条,锂是一种活泼的银白色金属。锂是最轻且最有正电性的金属之一,使其具有很高的反应活性。锂是电和热的良导体,熔点低(180 °C),柔软且有延展性。
应用
锂金属被广泛用于制造可充电电池的阳极材料,因为其负电化学电位低和理论比容量高。
警示用语:
Danger
危险声明
危险分类
Skin Corr. 1B - Water-react 1
补充剂危害
储存分类代码
4.3 - Hazardous materials which set free flammable gases upon contact with water
WGK
WGK 1
闪点(°F)
Not applicable
闪点(°C)
Not applicable
个人防护装备
Eyeshields, Faceshields, Gloves, type P3 (EN 143) respirator cartridges
法规信息
监管及禁止进口产品
Nanoscale, 5(17), 7890-7896 (2013-07-16)
Two-dimensional nanosheets can leverage on their open architecture to support facile insertion and removal of Li(+) as lithium-ion battery electrode materials. In this study, two two-dimensional nanosheets with complementary functions, namely nitrogen-doped graphene and few-layer WS2, were integrated via a
The Journal of organic chemistry, 78(17), 8274-8280 (2013-08-22)
An efficient one-pot synthesis of optically active β-alkyl-substituted alcohols through a tandem copper-catalyzed asymmetric allylic alkylation (AAA) with organolithium reagents and reductive ozonolysis is presented. Furthermore, hydroboration-oxidation following the Cu-catalyzed AAA leads to the corresponding homochiral γ-alkyl-substituted alcohols.
PLoS genetics, 9(3), e1003388-e1003388 (2013-04-05)
The number of chromosome sets contained within the nucleus of eukaryotic organisms is a fundamental yet evolutionarily poorly characterized genetic variable of life. Here, we mapped the impact of ploidy on the mitotic fitness of baker's yeast and its never
Advanced materials (Deerfield Beach, Fla.), 24(30), 4097-4111 (2012-04-17)
Two dimensional nanoarchitectures are of great interest in lithium storage for energy-storage devices, in particular lithium-ion batteries, due to its shortened paths for fast lithium ion diffusion and large exposed surface offering more lithium-insertion channels. Their competitive lithium-storage features provide
The journals of gerontology. Series A, Biological sciences and medical sciences, 69(7), 810-820 (2014-01-09)
Aging has been associated with the accumulation of damages in molecules and organelles in cells, particularly mitochondria. The rate of damage accumulation is closely tied to the turnover of the affected cellular components. Perturbing mitochondrial turnover has been shown to
我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.
联系技术服务部门