推荐产品
方案
≥99%
表单
liquid
折射率
n20/D 1.4454 (lit.)
沸点
144 °C (lit.)
密度
0.853 g/mL at 25 °C (lit.)
SMILES字符串
CC1CNCC(C)C1
InChI
1S/C7H15N/c1-6-3-7(2)5-8-4-6/h6-8H,3-5H2,1-2H3
InChI key
IDWRJRPUIXRFRX-UHFFFAOYSA-N
应用
3,5-Dimethylpiperidine was used to investigate the influence of substituents on heterocyclic piperidine as acid corrosion inhibitors for iron. It was used in the synthesis of pure phase ZSM-11 using extremely dense gels with minimal water contents.
Reactant for synthesis of:
Substituted bisphenol A derivatives as β-amyloid peptide aggregation inhibitors
MMP-13 selective isonipecotamide α-sulfone hydroxamates
Gem-diamines for active organocatalysts for biodiesel production
Benzimidazole inhibitors of the antigen receptor-mediated NF-κB
Reactant for Mannich reactions to form Ru(II) complexes
Substituted bisphenol A derivatives as β-amyloid peptide aggregation inhibitors
MMP-13 selective isonipecotamide α-sulfone hydroxamates
Gem-diamines for active organocatalysts for biodiesel production
Benzimidazole inhibitors of the antigen receptor-mediated NF-κB
Reactant for Mannich reactions to form Ru(II) complexes
警示用语:
Warning
危险分类
Eye Irrit. 2 - Flam. Liq. 3 - Skin Irrit. 2 - STOT SE 3
靶器官
Respiratory system
储存分类代码
3 - Flammable liquids
WGK
WGK 3
闪点(°F)
91.4 °F - closed cup
闪点(°C)
33 °C - closed cup
个人防护装备
Eyeshields, Faceshields, Gloves, type ABEK (EN14387) respirator filter
法规信息
危险化学品
Piperidines as corrosion inhibitors for iron in hydrochloric acid.
J. Appl. Electrochem., 34(7), 697-704 (2004)
Simple, efficient syntheses of zeolite ZSM-11 (MEL) at temperatures below 100? C using very dense gels.
Microporous and Mesoporous Materials : The Official Journal of the International Zeolite Association, 150, 7-13 (2012)